INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Aviation Fuel Thermal Properties

Aviation Fuel Thermal Properties

Aviation Fuel Thermal Properties

(OP)
Can anyone point me to a reference for the thermal properties of aviation fuel, specifically Jet A (JP8)? This is needed as I am involved in a design that will require the use of Jet A as a coolant.

RE: Aviation Fuel Thermal Properties

What properties?
See ASTM D 1655 for aviation turbine fuels Jet A or Jet A-1 with distallation, flash point, freeze point, viscosity, heat of combustion, smoke point, etc. and cross references to the testing standards for these properties.  Other ASTM specifications cover Jet B, Jet C-1 etc.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources