INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Blue Fin / Gold Fin vs Blygold?

Blue Fin / Gold Fin vs Blygold?

Blue Fin / Gold Fin vs Blygold?

(OP)
Hi all,
Is there anyone there with knowledge of the major differences between Blue Fin / Gold Fin anti-corrosive treatments vs Blygold?

I have heard Blue Fin / Golf Fin are a cheaper option but do not last as long as Blygold. Any idea of the price differences and/or the difference in durability?

Cheers
Jamo

RE: Blue Fin / Gold Fin vs Blygold?

Blygold is applied afterwards to the coil and needs to be maintained as well. For corrosion protection I would rather go for E-coating or cupper/cupper or aluminium/aluminium coils. In my opinion Blue fin/golf fin and Blygold are cheap solutions.

also see link.http://www.eng-tips.com/viewthread.cfm?qid=276080&page=1

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources