Determine C value of 1.25 Cr 0.5 Mo, as it applies to Larson-Miller
Determine C value of 1.25 Cr 0.5 Mo, as it applies to Larson-Miller
(OP)
I am trying to determine the "C" value of 1.25 Cr 0.5 Mo steel as it applies to the Larson-Miller Parameter. Can anyone point me in the right direction. Thank you.





RE: Determine C value of 1.25 Cr 0.5 Mo, as it applies to Larson-Miller
C=20
Source; EPRI