Anyone know of any mills that would be willing to hot roll a small quantity (10,000 lbs or less) of 1-9/16" square bar? The material needs to meet ASTM A350 Grade LF2 Class 1 specs. I am having a tough time finding anyone to do it. Hate to go oversees but I might not have a choice in this case (Hope I have not offended anyone). Any suggestions would be appreciated.
Thanks.
Thanks.





RE: HR Bar Stock made from ASTM A350
Scott Forge could be one option. They melt their own steel and can forge square bar. I believe they have supplied A/SA 350 steel. This would be a special order.