INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

WPS w/ one process qualified by a PQR 2 processes

WPS w/ one process qualified by a PQR 2 processes

WPS w/ one process qualified by a PQR 2 processes

(OP)
Dear All,

I'd like to request your help on the following subject:

 - I want to qualify a WPS for one process (GTAW)according to ASME IX, with a PQR for two processes (GTAW+SMAW). In the deposit metal thickness range t (QW-404.30) I've to apply the table QW-451, but for base metal thickness range T (QW-403.8) I've to put the same range of the deposit material t, or is better don't define?

thanks in advance

RE: WPS w/ one process qualified by a PQR 2 processes

Look at QW-256, essential variables for welding using the GTAW process.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources