INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Tapping 446 Stainless

Tapping 446 Stainless

Tapping 446 Stainless

(OP)
We are having problems tapping 446SS.  We are trying to tap 1/2" NPT in 1.125 Round Bar.  Can anyone suggest where I might be able to find information on tapping this material?  We have scrapped parts and our tooling salesman sent us a tap that they thought might work but it didn't.  

RE: Tapping 446 Stainless

(OP)
We were using a sulfur chlorinated compound made by Exxon but they have changed the formula recently.  We have always had trouble tapping this particular material for some reason...but this time it is really giving us a hard time.  We are going to order a different tapping compound as you suggest and see if that helps.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources