If I know the natural water content, max dry density, and the optimum water content of a soil, how do you calculate how much water needs to added to acheive optimum water content for a volume of soil? Thanks very much.





RE: Construction Water
2,000 x (0.18-0.12) = 100 pounds
That's how much water to add.
f-d
¡papá gordo ain't no madre flaca!