I am looking for a metal equivalent of 16mncr5.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
What is the metal equivalent of 16mncr5
|
RE: What is the metal equivalent of 16mncr5
thread330-34892: Equivalent to 16MnCr5 to sae steel