Looking for a material libriry for FEA
Looking for a material libriry for FEA
(OP)
Hi All,
Does anyone know a material library with temprature dependent properties for FEA?
What I need is very simple:
E: Elastic modulus V: Poisson's ratio
under different temperature.
We analysis plastics most of the time.
Thanks in advance.
Does anyone know a material library with temprature dependent properties for FEA?
What I need is very simple:
E: Elastic modulus V: Poisson's ratio
under different temperature.
We analysis plastics most of the time.
Thanks in advance.
Forever Young.....





RE: Looking for a material libriry for FEA
matweb.com
https://assist.daps.dla.mil/quicksearch/
http://www.knovel.com/web/portal/main
Also try on google books.
I have access to GE internal data bases if you want smth.