INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Aqua Ammonia Tank Vacuum Breaker Valve

Aqua Ammonia Tank Vacuum Breaker Valve

Aqua Ammonia Tank Vacuum Breaker Valve

(OP)
Hi,I'm looking for suggestions for a suitable Vacuum Breaker(s) for a 30,000 gal. stationary 29% Aqua Ammonia tank. We have had failures with Kunkle, Girard or DFT valves even though they are all 316 SS and suitable for ammonia service. I have looked at Johnson also, but this is located in an enviroment with up to 10 ppm SO2 concentration and the 440 SS ball is not suitable for SO2 service. 2-3" Hg rating would be a bonus.Any suggestions would be appreciated.Thanks  

RE: Aqua Ammonia Tank Vacuum Breaker Valve

It seems the previous breakers were made of metals.
Assuming the failures were due to corrosion

Suggestion 1: FRP or PVC Conservation vent (Groth)

Suggestion 2: FRP or plastic Water vent pot.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources