identify unusual steel composition
identify unusual steel composition
(OP)
Chromium 3.27
Carbon 0.41
Molybdenmum 0.96
Manganese 0.54
Ni .22, Si .21, V .19, Cu .25, Al .02
Remainder is iron
What is this grade? I have looked through all my referrence books, no luck with the chromium content.
Thanks in advance
Carbon 0.41
Molybdenmum 0.96
Manganese 0.54
Ni .22, Si .21, V .19, Cu .25, Al .02
Remainder is iron
What is this grade? I have looked through all my referrence books, no luck with the chromium content.
Thanks in advance





RE: identify unusual steel composition
What is the function of the steel component with this composition? This would help.
RE: identify unusual steel composition