INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Specification on the Freckles in the macrostructure of steel ingots

Specification on the Freckles in the macrostructure of steel ingots

Specification on the Freckles in the macrostructure of steel ingots

(OP)
I am looking for a specification relating to the freckles in the macrostructure inspection of steel ingots for forging and rolling parts for die molds.

What is acceptable an what is not acceptable for the freckles : size, shape, ....

Any Help
 

RE: Specification on the Freckles in the macrostructure of steel ingots

I think you're talking about macroetch/macrograph test standards.  If so check out:
ASTM E381 "Standard Method-Macroetch Testing...".
MIL-STD-430 "Macrograph Standards for Steel Bars, Billets, Blooms".
MIL-STD-1459 "Macrograph Standards for Steel Bars, Billets, Blooms...".

RE: Specification on the Freckles in the macrostructure of steel ingots

(OP)
Thanks Flesh

Actually i have made  macroetching of an ingot. I can not send the picture (confidential) i have small freckles but i don't know what is the right standard ?

For exemple here a macro etchning picture of a 35 tons ingot with freckles extracted from a book.

Is there any  numeric criteria  to accept or not the ingot related to the freckles ?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources