Do any of the North American codes state the minimum amount of time that a weld should sit for before NDE is performed? I believe it is either 24 or 48 hours. Please reference the applicable code.





RE: minimum amount of time before NDE
RE: minimum amount of time before NDE
517, and A 709 Grade 100 and 100W steels shall be
based on NDT performed not less than 48 hours after
completion of the welds.
RE: minimum amount of time before NDE
RE: minimum amount of time before NDE
Thank you
RE: minimum amount of time before NDE
RE: minimum amount of time before NDE
Hg
Eng-Tips policies: FAQ731-376: Eng-Tips.com Forum Policies