Charmille Surface finish
Charmille Surface finish
(OP)
Can anyone point me at a web page that gives equivalents between Charmille and other types of surface finish.
Thanks
Thanks
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Charmille Surface finish
Here is a good place to start.
http://www.mold-tech.com/tex/1tex.shtml
A Charmille finish is referenced when a certain texture is required when using the EDM (Electronic Discharge Machining) process.
Live Aloha
Frank M.
Tradewind Resources
http://www.tr-usa.com
RE: Charmille Surface finish
RE: Charmille Surface finish