INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

U-1A Form - Minimum Head Thickness

U-1A Form - Minimum Head Thickness

U-1A Form - Minimum Head Thickness

(OP)
Note 28 (Table W-3) for the minimum head thickness on line 8 of the manufacturer's data report states it is the "Specified minimum thickness of the head after forming.  It includes corrosion allowance."   
I would like to be sure it means the minimum head thickness specified (what is ordered) and not the calculated minimum thickness.  
Note 28 seems unambiquous, but nevertheless, I'm getting conflicting interpretation.

RE: U-1A Form - Minimum Head Thickness

Minimum head thickness refers to the specified minimum thickness of the supplied head (in the uncorroded condition).

It does not refer to any calculated value (what would be the point? Anyone can calculate the minimum required thickness once they have the material designation and the MAWP).


-Christine

RE: U-1A Form - Minimum Head Thickness

(OP)
Thanks for the response Christine.   
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources