INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Equivilant ASTM bar spec to A516?

Equivilant ASTM bar spec to A516?

Equivilant ASTM bar spec to A516?

(OP)
I am trying to specify the material for door handles and no stress lugs etc.

ASTM A516 is plate.  What is the equivilant for bar?  ASTM A675???

What is the spec for general purpose readily availible round and flat bar for vessel handles and attachments etc?

Thanks,

RE: Equivilant ASTM bar spec to A516?

You can specify A / SA-36 for non-pressure containing things as you described. Very common material.

jt

RE: Equivilant ASTM bar spec to A516?

I would go with the A/SA-36 as well, but if you are looking for equivalent strength, go with the 675.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources