INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

A36 steel corrosion rates

A36 steel corrosion rates

A36 steel corrosion rates

(OP)
Does anyone know where I can find corrosion rates for A36 steel in a severe marine environment?  

I have crevice corrosion between a clevis and gusset plate less than 1/4 mile from the ocean.  

Thanks,
Nick
 

RE: A36 steel corrosion rates

There are various sources for this information and it will depend on several factors - besides distance from the ocean, pollution (industrial)and location, location and location will effect the rate.

From ASM Handbook, Volume 13C

the rate of low carbon steel (similar to A 36) in a marine environment can vary from 0.53 mils/yr (rural) to 3.57 mils/yr (industrial), 5.73 mils/yr(mild) to 20 mils/yr (severe).
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources