ASTM A694 F60, looking for forging substitute in USA
ASTM A694 F60, looking for forging substitute in USA
(OP)
ASTM A694 F60 does not appear to be easily obtained in the USA. I'm looking for bar stock forging about 12" OD by 36" Long. Can anybody suggest an alternative?
Tensile yield = 60 ksi
Tensile strength = 75 ksi
Carbon Max = .30
Manganese Max = 1.5
Phosphorus Max = .030
Sulfur Max = .030
Silicon 0.13-0.37
The spec says ASTM A694 is used in high-pressure Transmission Service.
Design pressure = 5597 PSIG
Operating Temp = 120 F
Thank you,
Jonathan
Tensile yield = 60 ksi
Tensile strength = 75 ksi
Carbon Max = .30
Manganese Max = 1.5
Phosphorus Max = .030
Sulfur Max = .030
Silicon 0.13-0.37
The spec says ASTM A694 is used in high-pressure Transmission Service.
Design pressure = 5597 PSIG
Operating Temp = 120 F
Thank you,
Jonathan