Dear All,
One of My Client Specification refers stress relieving as Holding in 600 + or - 10 Deg C as per thickness requirement (say 1hour per inch thick) and cooling in still air without any controlled cooling.
In my opinion the Stress relieving will heating in a controlled way from 300 Deg C.
Holding in the 600 + or - 10 for the prescribed time
Cooling till 300 Deg C in controlled rate then cooling in still air.
Please clarify is there any practice like what i said above as per my client requirement.
One of My Client Specification refers stress relieving as Holding in 600 + or - 10 Deg C as per thickness requirement (say 1hour per inch thick) and cooling in still air without any controlled cooling.
In my opinion the Stress relieving will heating in a controlled way from 300 Deg C.
Holding in the 600 + or - 10 for the prescribed time
Cooling till 300 Deg C in controlled rate then cooling in still air.
Please clarify is there any practice like what i said above as per my client requirement.





RE: Stress Relieving
RE: Stress Relieving
RE: Stress Relieving