How Many A325 Bolts to Spot Check
How Many A325 Bolts to Spot Check
(OP)
Does anyone know the percentage of bolts to spot check on a structural steel building. Any tips will be greatly appreciated.
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
How Many A325 Bolts to Spot Check
|
How Many A325 Bolts to Spot CheckHow Many A325 Bolts to Spot Check(OP)
Does anyone know the percentage of bolts to spot check on a structural steel building. Any tips will be greatly appreciated.
Red Flag SubmittedThank you for helping keep Eng-Tips Forums free from inappropriate posts. Reply To This ThreadPosting in the Eng-Tips forums is a member-only feature.Click Here to join Eng-Tips and talk with other members! |
ResourcesThe world has changed considerably since the 1980s, when CAD first started displacing drafting tables. Download Now
Prototyping has always been a critical part of product development. Download Now
As the cloud is increasingly adopted for product development, questions remain as to just how cloud software tools compare to on-premise solutions. Download Now
Engineering-centric businesses face a number of challenges today, but unmanageable design and change processes don’t need to be counted among them. Download Now
|
RE: How Many A325 Bolts to Spot Check
RE: How Many A325 Bolts to Spot Check
RE: How Many A325 Bolts to Spot Check
RE: How Many A325 Bolts to Spot Check
http://www.FerrellEngineering.com
RE: How Many A325 Bolts to Spot Check
What type of connections are they; Slip critical, snug tight, pretensioned?
Is this an existing structure or are you checking the bolts during erection?
Check the recommendations of the RCSC for arbitration inspection. I believe you can get the RCSC on line.
Specification for Structural Joints Using ASTM A325 or A490 Bolts
It is like the Prego spaghetti sauce commercial - "It's in there."
Best regards - Al
RE: How Many A325 Bolts to Spot Check
Prior to installation, for pretensioned installation, a sample of not less than three assemblies of each type (diameter, length, grade, lot), shall be tested before installation.
During construction...
snug-tight connections - shall be visually inspected to verify that all plies are in firm contact.
pretensioned connections - RCSC requires "routine" observation of the installation method selected.
If it is determined after installation that proper pretensions have not be been obtained, additional procedures are given in the Arbitration section of RCSC.
Additional inspection guidelines can be provided within the contract documents.