F22 Class 1 v Class 3 & B16.5
F22 Class 1 v Class 3 & B16.5
(OP)
The B31.1, B31.3 piping codes plus ASME Section 2 list ASTM/ASME A182 Gr F22 in two classes, 1 and 3. There are different stress values given for the different classes
B16.5 and B16.34 give pressure / temperature ratings for only F22 Cl 3.
First...
has anyone encountered a ASTM A182 F22 Cl 1 valve or flange? I haven't yet found a supplier that will offer me Cl 1.
Second...
any guesses to why the B16 code committee excluded Cl 1?
B16.5 and B16.34 give pressure / temperature ratings for only F22 Cl 3.
First...
has anyone encountered a ASTM A182 F22 Cl 1 valve or flange? I haven't yet found a supplier that will offer me Cl 1.
Second...
any guesses to why the B16 code committee excluded Cl 1?
- Steve Perry