INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Material Properties 20 mil PVC Film Needed

Material Properties 20 mil PVC Film Needed

Material Properties 20 mil PVC Film Needed

(OP)
Hi All,

I need material properties, primarily tensile strength, on 20 mil thick pvc film used for boat and tent windows, seat covers etc.  This material is described as double polished, optically clear and cold crack resistant to -40 F

Can anybody help with tensile strength details?

Thanks
JQCF1

RE: Material Properties 20 mil PVC Film Needed

You can only get this information from the manufacturer or by testing the product. Flexible PVC is a formulated plastic with several ingredients which can vary between suppliers.  

RE: Material Properties 20 mil PVC Film Needed

Mfg is where the info might be found..Sometimes not??  Then find a new supplier.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources