Is it acceptable according to AWS D1.1?
Is it acceptable according to AWS D1.1?
(OP)
Dear Friends
Applicable Code - AWS D.1.1- Sect 4 Part B-Table 4.8.
In Module Skid Fabrication European Steel- S355JR, S275JR,A355JO used( Unlisted Material in AWS D.1.1).
Is it right/appropriate to use WPS/PQR Qualified using EH36 as base material?
If acceptable, pls advise ref. section of the code.
If not accepatable.what is the option? Require requalification?
Pls advise, Thanks.
Applicable Code - AWS D.1.1- Sect 4 Part B-Table 4.8.
In Module Skid Fabrication European Steel- S355JR, S275JR,A355JO used( Unlisted Material in AWS D.1.1).
Is it right/appropriate to use WPS/PQR Qualified using EH36 as base material?
If acceptable, pls advise ref. section of the code.
If not accepatable.what is the option? Require requalification?
Pls advise, Thanks.





RE: Is it acceptable according to AWS D1.1?
RE: Is it acceptable according to AWS D1.1?
If not, re-qualification of welds and welder is required.
http://www.FerrellEngineering.com
RE: Is it acceptable according to AWS D1.1?
Steve Jones
Materials & Corrosion Engineer
http://www.oilandgaspeople.com/cv/11499664