INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Thermal properties of S235JR and E295

Thermal properties of S235JR and E295

Thermal properties of S235JR and E295

(OP)
Hi
I'm looking for thermal properties of S235JR and E295 (Non-alloy structural steels).
Thermal conductivity and Specific Heat Capacity in particular.
Thanks for your help
  

RE: Thermal properties of S235JR and E295

Find a copy of ;
High Temperature Property Data: Ferrous Alloys
ed. Rothman, ASM, ISBN: 0-87170-243-6

They have them as graphs or I would list values.
All low alloy carbon steels have nearly identical physical properties.  The catch is finding a reliable source.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube

RE: Thermal properties of S235JR and E295

(OP)
Hi
Thanks for your reply.
I found the information from SolidWork 2009, but I was looking for an aternative source as the thermal conductivity for both material seems very low: 14 W/mK

Can someone comment on it?
Thanks

RE: Thermal properties of S235JR and E295

For carbon steel 1026, which would be similar to the steels listed above at 300 deg K

heat capacity @ 300 deg K ~ 0.48 kj/kg K

thermal conductivity @300 deg K ~ 52.4 W/m K

Source; Transport Phenomena in Materials Processing by Poirier and Geiger
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources