Allowable stress values per ASME B 31.1
Allowable stress values per ASME B 31.1
(OP)
According to ASME B31.1-2001 Article 102.3.1 (C),
"The basic for establishing the allowable stress values in this code are the same as those in the ASME Boiler and pressure vessel code, Section II, Part D, Appendix I".
My question is why allowable stress given in ASME B31.1 is UTS/4 not UTS/3.5 as given in ASME Section II part D ?
Thanks
Prasit
"The basic for establishing the allowable stress values in this code are the same as those in the ASME Boiler and pressure vessel code, Section II, Part D, Appendix I".
My question is why allowable stress given in ASME B31.1 is UTS/4 not UTS/3.5 as given in ASME Section II part D ?
Thanks
Prasit





RE: Allowable stress values per ASME B 31.1
I think the answer is that they are different Codes. Also B31.1 probably has not "aligned" with ASME VIII yet!!! Remember ASME VIII basis changed not too many years ago to UTS/3.5.
RE: Allowable stress values per ASME B 31.1
FAQ731-376: Eng-Tips.com Forum Policies