Waspaloy Properties
Waspaloy Properties
(OP)
Good DAy,
Im trying to find the way to get the best condition of foriging of waspaloy material... Does anyone knows the best way to forge this material without get cracks at the end of the process? Information about this material is also helpful...
Thank you!
Im trying to find the way to get the best condition of foriging of waspaloy material... Does anyone knows the best way to forge this material without get cracks at the end of the process? Information about this material is also helpful...
Thank you!





RE: Waspaloy Properties
htt
RE: Waspaloy Properties
Kind Regards
RE: Waspaloy Properties
I know we had a very hard time getting a turbine disc forged as it was a one off design and one off part.. We did order the second one before they forgot how they forged the first one.
I would check with Carpenter for information available to the public.
ht
RE: Waspaloy Properties
Mr. Unclesyd,
Thank you for your information is very helpful and I would appreciate any extra-data you can share about these kind of materials.
Kind Regards,
RE: Waspaloy Properties
http://www.cartech.com/techarticles.aspx?id=1662
Another is a booklet called "Forging Quality Stainless Steel & High Temperature Alloys". You can request that it be sent to you using the following link:
http://www.cartech.com/productliterature.aspx
RE: Waspaloy Properties
Forging Waspaloy isn't for the faint of heart.
http:
RE: Waspaloy Properties
http:/
RE: Waspaloy Properties
Regards,
Luis P
RE: Waspaloy Properties