INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Concrete slump requirements (lower and upper limits) per ACI!

Concrete slump requirements (lower and upper limits) per ACI!

Concrete slump requirements (lower and upper limits) per ACI!

(OP)
Is there a section or table in ACI that shows the slump limits? I would appreciate it.

RE: Concrete slump requirements (lower and upper limits) per ACI!

See ACI 211 Table 6.3.1 "Recommended Slumps for Various Types of Construction" and ACI 117 Section 2.5.1.  

Greg

RE: Concrete slump requirements (lower and upper limits) per ACI!

Once a recommended slump has been selected and specified, the limits of the delivered slump range are then defined in ASTM C94, paragraph 6.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources