INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

da/dan Mil-HDBK-5

da/dan Mil-HDBK-5

RE: da/dan Mil-HDBK-5

No. For 6061-T6 it has S-N data for Kt = 1.0.

Like IRstuff, I do suspect that once a question is even three months old any answer is pointless, though it does seem a little cruel that no one could be bothered to put  doncrawford  out of his misery at the time.

Just in case poor old  doncrawford  is still waiting:

Code    M6AB13AB1
YS    41
UTS    45
KIe    36
K1c    26
Ak    1
Bk    0.75
C    9.00E-08
n    2.3
p    0.5
q    0.5
DKo    3.5
C+th    1.5
C-th    0.1
Rcl    0.7
a    2
S.R.    0.3
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources