INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

302 and 304 stainless steel sigma-eps graph

302 and 304 stainless steel sigma-eps graph

302 and 304 stainless steel sigma-eps graph

(OP)
where can i get sigma-eps graph for those two (302, 304) stainless steels, not annealed or hardened in any other way?
is there anything in those MIL handbooks? which one?

RE: 302 and 304 stainless steel sigma-eps graph

MIL-HDBK-5 and its replacement DOT/FAA/AR-MMPDS have stress strain curves for Type 301 stainless steel in the cold-rolled condition (1/4 hard, 1/2 hard, and full-hard).  Type 302 is essentially the same composition as 301, but 302 is for wire applications while 301 is for sheet.  I'm sure a Google search would find something on this topic.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources