Why tensile test Fail?
Why tensile test Fail?
(OP)
Dear Sir,
FYI, we run a several test for our LF2 material.
Charpy test at -46C- pass
Hardness test- average is 140HV
Tensile test- average is 450Mpa(requirment is 485Mpa).
Anybody can explain what the reason we failed the tensile test?
Thanks
FYI, we run a several test for our LF2 material.
Charpy test at -46C- pass
Hardness test- average is 140HV
Tensile test- average is 450Mpa(requirment is 485Mpa).
Anybody can explain what the reason we failed the tensile test?
Thanks