INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Large Diameter super-duplex heads.

Large Diameter super-duplex heads.

Large Diameter super-duplex heads.

(OP)
I have a need for some large diameter super duplex head that will have to be manufactured in two (2)welded together prior to forming.  Our suppliers here can not get the plates to quenching fast enough after annealing so the welds will be crack sensitive.   Where do you guys buy these large diameter  120" to 156" i.d.  2:1 elliptical.

RE: Large Diameter super-duplex heads.

(OP)
none of these can do it

we have gone to anonius in the netherlands

and brighton with an alternate of AL6XN

RE: Large Diameter super-duplex heads.

Did you try Europe ( France, Italy, Spain, Belgium) for diameters to 4.2 m made of Uranus 52 N?
Also, a couple of major Indian suppliers could help you, same Uranus 52 N or even 2507.
Thickness to 5" in Spain.
Caution;- dished end forming of this material would invariably force you to compromise the theoretical shape, so be prepared.
Cheers,
gr2vessels

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources