Cryogenic use of alloy type 625 (UNS N06625) & 825 (UNS N08825)
Cryogenic use of alloy type 625 (UNS N06625) & 825 (UNS N08825)
(OP)
Could somebody please indicate how to find information related to the use of Nickel-Base alloy type 625 (UNS N06625) and type 825 (N08825) in cryogenic conditions.
There are some literature where the mechanical properties of this alloys at low temperatures are described?
Many thanks
There are some literature where the mechanical properties of this alloys at low temperatures are described?
Many thanks





RE: Cryogenic use of alloy type 625 (UNS N06625) & 825 (UNS N08825)
RE: Cryogenic use of alloy type 625 (UNS N06625) & 825 (UNS N08825)
http://www.weibull.com/knowledge/milhdbk.htm
RE: Cryogenic use of alloy type 625 (UNS N06625) & 825 (UNS N08825)
http
lists some properties at low temps. The impacts look good all of the way down.
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube