what does GRIDS mean??
what does GRIDS mean??
(OP)
Hello:
I am new in this, so i dont know if i did it well
According with tubes & pipes, there a measure of POLISHING called GRIDS.
What does it mean?? Where can i find something of that??
Is 150grids a hight grade of polish or low grade??
How can i estimate how many grids a process needs??
Thanks and i look forward for an answer
I am new in this, so i dont know if i did it well
According with tubes & pipes, there a measure of POLISHING called GRIDS.
What does it mean?? Where can i find something of that??
Is 150grids a hight grade of polish or low grade??
How can i estimate how many grids a process needs??
Thanks and i look forward for an answer





RE: what does GRIDS mean??
See this link:
http://en.wikipedia.org/wiki/Sandpaper
RE: what does GRIDS mean??
For sand paper, 40-80 grit would be very rough sanding material.
In my opinion, 150-180 would be medium and 240 grit or higher would be for fine polishing.
Grinding wheels (molinar) are rated by grit also.
rmw