Steel prices for fabricators - Where?
Steel prices for fabricators - Where?
(OP)
Dear Eng-Tipers,
Happy New Year to all. I am looking for prices of carbon steel to fabricate pressure vessels. Where could I get this information at low cost (or, preferably, free.)
TIA
Happy New Year to all. I am looking for prices of carbon steel to fabricate pressure vessels. Where could I get this information at low cost (or, preferably, free.)
TIA





RE: Steel prices for fabricators - Where?
right now as rolled sa-516-70 is now 35.00 CWT for plate on the Texas Gulf Coast.
RE: Steel prices for fabricators - Where?
Thanks.
Sure. CWT. Short, long, metric? Care to clarify?
Regards,
RE: Steel prices for fabricators - Where?