BS1501 - 161/151 grade 400A
BS1501 - 161/151 grade 400A
(OP)
Hi
Can anyone please explain the designation of: BS1501 - 151/161 grade 400A? What does the 151/161 stand for?
Regards
Jim
Can anyone please explain the designation of: BS1501 - 151/161 grade 400A? What does the 151/161 stand for?
Regards
Jim





RE: BS1501 - 161/151 grade 400A
161 = Si Killed
Suggest you get a copy of the standard
RE: BS1501 - 161/151 grade 400A
Regards
athomas236