H2SO4 AT LOW CONCENTRATION
H2SO4 AT LOW CONCENTRATION
(OP)
Hello,
I have a commodity with a concentration of 0,5% of H2S04 and a temperature of 200ºC, and, I don't know if this concentration is very acid.
Someone can help me??
Thanks,
I have a commodity with a concentration of 0,5% of H2S04 and a temperature of 200ºC, and, I don't know if this concentration is very acid.
Someone can help me??
Thanks,





RE: H2SO4 AT LOW CONCENTRATION
One needs a little more information to give any advice.
Is the 0.5% based on vol or weight?
What form is the commodity?
What are the other ingredients?
What do you hope to accomplish?
RE: H2SO4 AT LOW CONCENTRATION
0,5% vol; liquid; water.
I have to specify the material of piping.
Thanks,
RE: H2SO4 AT LOW CONCENTRATION
Look here for good tips
http://
I would suggest that you look at duplex stainless grades, but you are going to need a high alloy material for any real durability at that temperature.
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
RE: H2SO4 AT LOW CONCENTRATION
here you can find some help to select the correct material
http:/
S
Corrosion Prevention & Corrosion Control
RE: H2SO4 AT LOW CONCENTRATION
Please find a iso corrosion diagram on page 5 in the attached material data sheet.
RE: H2SO4 AT LOW CONCENTRATION