INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

U stamp certified closures for A694 F65 material welded to API X65

U stamp certified closures for A694 F65 material welded to API X65

U stamp certified closures for A694 F65 material welded to API X65

(OP)
several vendors have issues with providing U stamp certified closures for A694 F65  material welded to API X65 barrel material.

could someone enlighten me if there is any issue with ASME Ustamp for the proposed material combination

RE: U stamp certified closures for A694 F65 material welded to API X65

The materials are not listed under ASME II; thus, they cannot be stamped unless the materials are covered under a Code Case.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources