low temperature fatigue of hdpe
low temperature fatigue of hdpe
(OP)
I'm looking for fatigue data for hdpe at about -45C (-50F). Seems to be a lot of data at and above RT, but little at low temperatures. Can anyone help?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
low temperature fatigue of hdpe
|
RE: low temperature fatigue of hdpe
Chris DeArmitt
www.phantomplastics.com
Consulting to the plastics industry
RE: low temperature fatigue of hdpe
I would ask Borealis if they had data
Regards
Pat