INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Anti-Graffiti Coatings for Concrete

Anti-Graffiti Coatings for Concrete

Anti-Graffiti Coatings for Concrete

(OP)
We are designing a bridge and the client has requested that all vertical concrete surfaces be coated to prevent graffiti. We have not specified this before, but from looking on the internet, I see there are sacrificial and permanent coatings available.

Anyone have any experience with either?  Recommendations on which type is better?

Thanks

RE: Anti-Graffiti Coatings for Concrete

One solution is,that you contact a few supliers of anti graffiti coating. Than you have 'll have a clear what is usefull for your applience. and what is on the market.

 

Signature: I'm dutch and I'll  do my best on my English;)

RE: Anti-Graffiti Coatings for Concrete

I was marginally involved on the selection of an antigraffiti coating on a previous job, in fact some elements were 'marked' before constructio finished. We could not find anything really effective. All treatments were really temporary and involved regular re-application and strong power washing and scrubbing to remove the graffiti anyway.

Finaly we opted for not doing anything and paint over the graffiti with a concrete colour paint immediately after it would be discovered. Apparently the artist loose interest if after spending a considerable amount of time the 'art' is covered next morning without anybody seeing it.

I would be interested if you find anything effective though. I could use it on future jobs
 

RE: Anti-Graffiti Coatings for Concrete

Ever hear about how the media boosted the proliferation of grafitti in NYC?

A TV newscaster once highlighted grafitti, and the grafitti kids responded in droves hoping to be featured on TV.

I would like to hear about how NYC finally brought this to a screeching halt.  Jail time and bills to the parents probably helped.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources