INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Factored weld resistance of 1/4" fillet weld with stainless

Factored weld resistance of 1/4" fillet weld with stainless

Factored weld resistance of 1/4" fillet weld with stainless

(OP)
Would any one know what is the factored weld resistance of a 1/4" fillet weld between stainless Grade 304 material?  Where would be a resource I could look this up?  What electrode classification number is generally used?

RE: Factored weld resistance of 1/4" fillet weld with stainless

Google " welding stainless steel " .  A resource that should pop up is a NIDI publication that has all you want including the strength listings for all types of weld rod and processes.

rmw

RE: Factored weld resistance of 1/4" fillet weld with stainless

Recommended electrode for 304 to 304 welds is AWS A5.9, ER308L, not that this is the only electrode that can used.

"Saving the World One Beam at a Time"

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources