INTELLIGENT WORK FORUMS FOR ENGINEERING PROFESSIONALS
Come Join Us!
- Talk With Other Members
- Be Notified Of Responses
To Your Posts
- Keyword Search
- Turn Off Ad Banners
- One-Click Access To Your
Favorite Forums
- Automated Signatures
On Your Posts
- Best Of All, It's Free!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.
Partner With Us!
"Best Of Breed" Forums Add Stickiness To Your Site

(Download This Button Today!)
Member Feedback
"...Your site is one of the cleanest and BEST forums that I
have seen. I have sent quite a few people your way. Keep up
the good work!!!"
Geography
Where in the world do Eng-Tips members come from?
|
Compress forcing normalization of flange in Appx 1-6
|
|
BigTank (Mechanical) |
26 Oct 09 14:36 |
I'm designing a dished cover with a bolting flange like Fig. 1-6 sketch D (Appendix 1-6). I cannot find in the code where SA-516 Gr. 70 material used for the flange must be normalized (at 3-1/4 thick), but Compress keeps forcing it. Please help me find this in the code! It's driving me CRAZY! -------------------------------- Fitter, happier, more productive |
|
i think that any plate that thick requires normalizing for asme code |
|
BigTank,
It is in the material spec. for SA-516...Section 5.2 which says,
"Plates over 1.50 in. [40 mm] in thickness shall be normalized." |
|
|
BigTank (Mechanical) |
26 Oct 09 15:14 |
thanks doct...i was just logging in to post that i found that information myself. man, sometimes chasing stuff down can be frustrating! thanks, gents! -------------------------------- Fitter, happier, more productive |
|
|
 |
|