Compress forcing normalization of flange in Appx 1-6
Compress forcing normalization of flange in Appx 1-6
(OP)
I'm designing a dished cover with a bolting flange like Fig. 1-6 sketch D (Appendix 1-6). I cannot find in the code where SA-516 Gr. 70 material used for the flange must be normalized (at 3-1/4 thick), but Compress keeps forcing it.
Please help me find this in the code! It's driving me CRAZY!
Please help me find this in the code! It's driving me CRAZY!
--------------------------------
Fitter, happier, more productive





RE: Compress forcing normalization of flange in Appx 1-6
RE: Compress forcing normalization of flange in Appx 1-6
It is in the material spec. for SA-516...Section 5.2 which says,
"Plates over 1.50 in. [40 mm] in thickness shall be normalized."
RE: Compress forcing normalization of flange in Appx 1-6
man, sometimes chasing stuff down can be frustrating!
thanks, gents!
--------------------------------
Fitter, happier, more productive