INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Duplex2205 Torquing

Duplex2205 Torquing

Duplex2205 Torquing

(OP)
I m looking for a table or a Spec. with the bolt torque and bolt force values (Friction coefficient U= 0.10 to =.12).

Material: Duplex 2205 (UNS S32205- ASTM 479)

Target. To fix an structure cell.

I found nothing in Codes, nothing in google........ May be here, get it.

Thanks
 

RE: Duplex2205 Torquing

(OP)
Hi Steve., finally we are using the same Troque table for ss316. Thanks You

RE: Duplex2205 Torquing

How about sharing some torque numbers with others..?

   

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources