I just recently had a part chemically analyzed to verify that is it AL6061 (ASTM B221)
The lab results came back and it was actually AL6162.
I tried to find mechanical properties of this alloy but could not find a single thing.
Has anyone come across this alloy before? Is it better than 6061? Where can I find mechanical properties for it?
thanks in advance.
I just recently had a part chemically analyzed to verify that is it AL6061 (ASTM B221)
The lab results came back and it was actually AL6162.
I tried to find mechanical properties of this alloy but could not find a single thing.
Has anyone come across this alloy before? Is it better than 6061? Where can I find mechanical properties for it?
thanks in advance.





RE: whats is AL6162
http://en
www.matweb.com
RE: whats is AL6162
After more digging, I actually found some info.
Here is the link for future forum use.
http://yuansheng.com/properties/6000_alloys.htm