INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Need source/info for Vanox

Need source/info for Vanox

Need source/info for Vanox

(OP)
I'm looking for the manufacturer of a material called Vanox. One website for bicycle saddles describes Vanox as:

Vanox is a proprietary alloy composite of stainless steel, titanium and vanadium, made in Germany. It is an ideal alloy for saddle rails because of its durability (not subject to stress riser -- where the sharp end of an unmitered seatpost cradle has been known to cause titanium rails to break) and is actually lighter than regular titanium rails (not tubular titanium, which is lighter yet). It's less prone to failure, is lighter and is slightly less expensive than all-titanium rails.

Thanks,
Don Culp
 

RE: Need source/info for Vanox

Selle Italia SRL holds the trademark in Europe for Vanox.  The description you quote was written by someone who is not an expert on metals.  This is not a composite, it is a steel alloy.  I don't know who makes this, but I imagine it is a German stainless steel wire producer.  Here is a list:

http://www.stahl-online.de/stahl_zentrum/mitgliedsunternehmenEdelstahl.asp

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources