INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Agma 8-CH-13 quality designation
2

Agma 8-CH-13 quality designation

Agma 8-CH-13 quality designation

(OP)
I have a gear drawing with "Quality 8-CH-13" designation. I suppose the quality class required is 8, but what does the 13 stand for?
 

RE: Agma 8-CH-13 quality designation

Just a guess. But if CH means Carburized & Hardened then the 8 could be the quality before CH and the 13 could be the quality after CH. Often the process is to hob the gear, heattreat it, and then finish grind.

RE: Agma 8-CH-13 quality designation

2
never guess

the Q-8 CH 13

The CH 13 = alloysteel carburized 55 HRc min

AGMA 2000-A-88 Page 24 & AGMA 240

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources