Friction Coefficients
Friction Coefficients
(OP)
Gents,
I was just wondering your opinions/any good refrence material you know of on the friction co-efficients of some of the following:
Steel - PTFE
Steel - Concrete (Wet or underground)
Steel - Conrrete (dry)
I have had a look around the net and found a few bits but nothing conclusive.
Thanks in advance!
PST
I was just wondering your opinions/any good refrence material you know of on the friction co-efficients of some of the following:
Steel - PTFE
Steel - Concrete (Wet or underground)
Steel - Conrrete (dry)
I have had a look around the net and found a few bits but nothing conclusive.
Thanks in advance!
PST






RE: Friction Coefficients
http
http://www.supercivilcd.com/FRICTION.htm
So it seems with teflon under .1 and much lower and steel-concrete no less than .45 just in case.
RE: Friction Coefficients