304SS flange mated to 3-1/2Ni flange.
304SS flange mated to 3-1/2Ni flange.
(OP)
I have a Manway cover that is a 20" 300# blind made of SA-350-LF3 (3-1/2 Ni) steel that needs a new manway cover.
There is a long delivery on a new 3-1/2 Ni manway cover, but I can get a 304SS manway cover off the shelf. The 304SS is acceptable for the cold service. I would have to mate it to the existing 3-1/2 Ni flange that is currently on the manway nozzle.
Before I make the change I want to ensure that there will not be any potential problems. Has anyone ever mated a 304SS blind flange with a 3-1/2 Ni flange?
I would appreciate it if anyone can point out any potential problems.
There is a long delivery on a new 3-1/2 Ni manway cover, but I can get a 304SS manway cover off the shelf. The 304SS is acceptable for the cold service. I would have to mate it to the existing 3-1/2 Ni flange that is currently on the manway nozzle.
Before I make the change I want to ensure that there will not be any potential problems. Has anyone ever mated a 304SS blind flange with a 3-1/2 Ni flange?
I would appreciate it if anyone can point out any potential problems.





RE: 304SS flange mated to 3-1/2Ni flange.