INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

what is 40Cr10 Material

what is 40Cr10 Material

what is 40Cr10 Material

(OP)
  
Dear,
     It is my first question in this Forum, we are saw pipe manufacture and for expander machine we require to develop different size of tools for respective size of pipe, our technical people are asking me to use 40cr10 material for these types of tool. I do not have much more information about this material so please if any body have any idea about it then reply for following queries.

What is 40Cr10 Material? Is it tool steel, Die steel or low alloy steel? Which heat treatment is good for this type of material?
 

RE: what is 40Cr10 Material

40Cr10 is Romanian standard. its American equivalent is 5140 and material number is 1.7035

in key to steel book it is categorized as Structural and constructional steels.

the heat treatment depends on what you expect from this material.

hope it helps.
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources