INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

PET GMT plate supplier

PET GMT plate supplier

PET GMT plate supplier

(OP)
Does anyone know of european supplier for extruded plates in PET- glassfiber (GMT prepreg material)?

RE: PET GMT plate supplier

There are various manufacturers of glass fabric/thermoplastic matrix sheets. Most products are PP, PA, PU and PPS. See Twintex (from Vetrotex), Versitex, Cetex and Tepex (you recognize these products by their name, they all end up by "tex").

In PET, the only I saw in the past (in a conference, so I'm not sure they have the commercial product) was made by Polystrand.
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources